3M™ Scotch-Weld™ Epoxy Adhesive 7240 FR

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M™ Scotch-Weld™ Epoxy Adhesive 7240 FR

Main features

  • Long open time for large surface application
  • Non-sag properties
  • Contains glass beads for thickness control

Product Description

3M™ Scotch-Weld™ Epoxy Structural Adhesive 7240 B/A FR is a two-part, 2:1 mix ratio adhesive and contains glass beads for control of minimal bond line thickness.

Product Key Features

  • Long open time for large surface application
  • Non-sag properties
  • Contains glass beads for thickness control
  • High resistance to environmental exposure
Product Family

3M-7240FR/BLK400MLAM

Black, US/Canada Label, 400mL Duo-Pak, 6 Each/Case
1. Select Package Type
2. Select Color

Loading pricing…

Product availability
EU Shipping in 2 weeks
Packaging
Unit of measure Cartridge
Net weight 0.652383 kg
Gross weight 0.652383 kg
Dimensions 4.61 x 2.57 x 12.08 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Modified Amine/Modified Epoxy
Color
The color
White/Black
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
1 hours

Leading Brands Trust in Our Products and Services