3M™ Scotch-Weld™ Low Odor Acrylic Adhesive DP810

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M™ Scotch-Weld™ Low Odor Acrylic Adhesive DP810

Main features

  • Tough, durable bonds
  • Minimal surface prep
  • Excellent shear and peel strength

Product Description

3M™ Scotch-Weld™ DP810 Low Odor Acrylic Adhesives is a two-part, 1:1 mix ratio, toughened structural adhesive with less odor than most acrylic adhesives. DP810 has excellent shear and peel strength along with good impact resistance and durability. It can quickly bond to most metals, ceramics, rubbers, plastics and wood with minimal surface preparation.

Product Key Features

  • Tough, durable bonds 
  • Low odor acrylic adhesive
  • Minimal surface prep
  • 10-minute work life
  • 20-minute time to handling strength
  • 1:1 mix ratio
  • Excellent shear and peel strength
  • Bonds stainless steel
Product Family

3M-DP810/ST48.5ML

48.5 ml, Skin Tone
1. Select Package Type
2. Select Color

Loading pricing…

Product availability
EU Shipping in 2 weeks
Packaging
Unit of measure Cartridge
Net weight 0.0739 kg
Gross weight 0.0739 kg
Dimensions 4.61 x 2.57 x 12.08 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Acrylic
Color
The color
Green/White
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
1:1
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
0.17 hours
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
18,000 - 22,000 mPa.s