LOCTITE ABLESTIK ICP 8118

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK ICP 8118

Main features

  • Snap cure
  • Excellent flexibility
  • High speed dispensing

Product Description

LOCTITE ABLESTIK ICP 8118  is an electrically conductive adhesive designed for applications that require a very fast cure at low temperatures. It is ideally suited for high throughput photovoltaic dispense processes and applications where high adhesion strength is desired. Low and stable contact resistance is achieved on noble metallization during reliability testing.

LOCTITE ABLESTIK ICP 8118 is a single component acrylate that displays excellent flexibility and is typically used for flexible interconnect in photovoltaic shingle applications.

 

Snap Cure

  • 10 to 15 seconds @ 150°C
Product Family

ICP8118/10C0

10cc Syringe - 2386251
1. Select Package Type

Loading pricing…

Packaging
Unit of measure Syringe
Net weight 15 g
Gross weight 24 g
Dimensions 3 x 2.3 x 9.1 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.9
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
0.004 Ohms⋅cm

Additional Information

Protip
By applying a flat and thin 100-200um layer using JET dispensing or STENCIL printing (instead of one domed dot), we believe that the flow out and bleeding can be reduced by lower gravity forces.