LOCTITE ABLESTIK JM7000
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Low moisture in cavity
- Low ionic impurities
- Minimal voiding
Product Description
LOCTITE ABLESTIK JM 7000 die attach adhesive has been formulated for use in high throughput die attach applications and hermetic packages. This material has been used successfully on rigid substrates with die sizes up to 700 mils. LOCTITE ABLESTIK JM 7000 is very stable in high temperatures and has been approved by DESC and Rome Laboratory for military products.
LOCTITE ABLESTIK JM7000 is a cyanate ester, solvent-containing formulation so it will behave similarly to other Cyanate ester products.The degradation temperature, otherwise known as Onset decomposition temperature provided by the TGA for almost identical products shows decomposition of 0.3% at 400°C so JM7000 should be affected in a similar manner.
Typical Cure Schedule
- 30 min @ 150°C
For applications that require higher electrical conductivity, a cure cycle of 15min @ 300°C is recommended.
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Physical Properties
Additional Information

These products are old and so is the data accompanying them. Here is a TGA scan on an already cured JM7000 sample that shows that as the temperature increases the polymer starts to break down. Adhesion strength will start to decrease as the temperature increases approximately past 300°C and it's possible that this weight loss is indication of outgassing or decomposition. Please check the Technical documents section for a new(er) and full(er) data package.