Aculon 73DE Offset
Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated
Main features
- Fluorinated Solvent
- Heavy duty vapor degrease
- 3M Novec 73DE alternative
Product Description
Aculon 73DE Offset is a clear fluorinated solvent blend designed for heavy-duty vapor degreasing or immersion cleaning applications. Some of the features include high solvency, low surface tension, non-flammability, and fluid stability.
Vapor degreasing with Aculon 73DE fluid can help save time and costs over by offering faster cycle times, lower energy usage, and improved cleaning of parts with complex geometries. It is a direct replacement for Novec 73DE.
Key Features
- Effective in cleaning heavy greases, oils, waxes, silicones, and non-polar flux residues.
- Easy maintenance and use in a vapor degreaser with stable bath composition during extended use.
- Non-flammable and low in toxicity.
- Environmentally sustainable with low global warming potential (GWP) and 0 ozone depletion potential(ODP).
- Replacement for Novec 73DE, nPB, TCE, ozone-depleting HCFCs, and high GWP HFCs.
- Effective for lubricant deposition applications where increased solvency is desired.
Packaging
Unit of measure Pail
Net weight 25 kg
Gross weight 27.5 kg
Dimensions 28 x 30 x 37 cm
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Appearance
clear/colorless
Appearance at room temperature.
Solids
none %
Specific Gravity
1.28
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume.
For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
Vapor Pressure
0.36 kg/cm2
Thermal Properties
Boiling Point
48 °C
The amount of degree’s needed to reach in order to make the substance boil.
Physical Properties
Viscosity
1 mPa.s
Viscosity is a measurement of a fluid’s resistance to flow.
Viscosity is commonly measured in centiPoise (cP). One cP is defined as
the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP.
A product like honey would have a much higher viscosity -around 10,000 cPs-
compared to water. As a result, honey would flow much slower out of a tipped glass than
water would.
The viscosity of a material can be decreased with an increase in temperature in
order to better suit an application
Additional Information
Aculon 73DE Offset vs 3M Novec 73DE
| 3M Novec 73DE | Aculon 73DE | |
| Viscosity (cP) | 0.38 cP | <1 cP |
| Liquid Density (g/mL) | 1.28 | 1.28 |
| Boiling point (°C) | 48 | 48 |
| Surface Tension (dynes/cm) | 19.9 | 19.9 |
| Kauri-Butanol Value | 83 | 83 |
| Vapor Pressure (mm/Hg @ 20 °C) | 263 | 263 |
| Heat of Vaporization (cal/g @ boiling point) |
54.2 | 54.2 |
| Shelf life | 2 years | 2 years |
Aerospace Materials Compatibility
| Test Description | ASTM Method | Test result |
| Sandwich Corrosion | F1110 | Passes |
| Effect on Painted Surfaces | F502 | Passes |
| Hydrogen Embrittlement | F519 | Passes |
| Effect on Unpainted Surfaces | F485 | Passes |
| Total Immersion Corrosion | F483 | Passes |
| Low-Embrittling Cadmium Plate | F1111 | Passes |
| Flash Point | D56 | Passes |
| Acrylic Stress Crazing | F484 | Does Not Pass |
| Stress Corrosion of Titanium Alloys | F945 | Passes |
Compatibility with Materials
| Plastics | Compatible | Acetal, Epoxy, Nylon, PEEK, Polyester, Polyethylene, Polypropylene, PTFE |
| Plastics | Incompatible | ABS, Polystyrene, Acrylic, Polycarbonate |
| Elastomers | Compatible | DuPont Kalrez Perfluoroelastomers, Butyl Rubber, Parfluor Perfluoroelastomers, Viton Fluoroelastomers, Polyurethane |
| Elastomers | Incompatible | Silicone, Fluorosilicone |
| Metals | Compatible | Copper, Brass, Stainless Steel, Magnesium, Titanium, Aluminum, Carbon Steel, Cadmium |
| Metals | Incompatible | No Data |