Spectracarb 2050A | Graphitized Carbon Fiber GDL Sheets

Harmonization Code : 6815.11.00.00 | Articles of stone or of other mineral substances, not elsewhere specified or included; Non-electrical articles of graphite or other carbon; Carbon fibres and articles of carbon fibres

Spectracarb Graphitized Carbon Fiber GDL Sheets Spectracarb 2050A | Graphitized Carbon Fiber GDL Sheets Spectracarb 2050A Series Graphitized Carbon Fiber GDL Sheets

Main features

  • Spectracarb 2050A - Multiple grades
  • Gas Diffusion Layer Sheets
  • Discontinued Q4 2020

Product Description

Spectracarb™ product line has been discontinued since 2020.

CAPLINQ has developed LINQCELL™ Carbon Fiber Paper GDL a better and more cost-effective alternative

 

Spectracarb™ 2050A Gas Diffusion Layer (GDL) sheets are sometimes called porous carbon gas diffusion layer. They are porous graphitized resin-bonded carbon fiber papers and multi-ply panels specifically designed for use in PEM, DMFC and PAFC fuel cells, Electrolyzers, Humidifiers and Other Electrochemical Devices.

Spectracarb 2050A Series Porous Graphitized Sheets and Panel

Spectracarb™ 2050A Porous Carbon Gas Diffusion Layer (GDL) sheets are porous graphitized resin-bonded carbon fiber papers and multi-ply panels specifically designed for use in PEM, DMFC and PAFC fuel cells, Electrolyzers, Humidifiers, and Other Electrochemical Devices

These products are optimized for the following properties:

  • Electrical Conductivity
  • Mechanical Strength and Durability
  • Gas/Air Permeability
  • Water Management

Spectracarb GDLs are produced in the USA and are available in a wide range of standard and custom grades, densities, sizes and materials for fuel cells, electrolyzers, humidifiers, specialty batteries and other electrochemical applications.

Advantages of EFT Fibers' Spectracarb Series GDLs

Spectracarb GDL has a specific technology focus:

  • Widest Range of Production Grades Available
  • Lower Cost Products
  • Small / Specialty Orders Accepted
  • Experimental & Developmental Formulations (Laboratory /Pilot Scale)
  • Contract Research /Joint Development Programs for Special Requirements
  • Established 22-Year Manufacturing History (Spectracorp Founded 1991)

Spectracarb GDL 2050 Series Sizes, Thicknesses, and Densities

The Spectracarb 2050 Series GDL sheet sizes are 55 x 55 cm. Custom sizes, machined discs, and other customer-defined sizes and shapes, as well as channels and surface grinding, are available upon request for large quantities.

 

 

Product Family

2050A-0850

7.5 mil (190micron) thick x 0.50g/cc density x 40cm x 40cm sheet

Loading pricing…

Technical Specifications

General Properties
Porosity
Void fraction is a measure of the void spaces in a material
78 %

Additional Information

Spectracarb product line has been discontinued since 2020.

KRAYDEN has developed LINQCELL a better and more cost-effective alternative

Graphitized Carbon Fiber Papers and Plates for GDL
Product Thickness Thickness (mm) Density (g/cm3) Basis weight (g/m2) Through-Plane Resistance (mΩcm2) Through-Plane Resistivity (mΩcm) Voltage Loss (mV)
LINQCELL GDP 180 0.007" 0.18 -  50 7 - -
LINQCELL GDP 210 0.008" 0.21 - 51 10 - 14
LINQCELL GDP 240 0.009" 0.24 - 90 15 - -
LINQCELL GDP 340 0.013" 0.34 - 90 10 - -
LINQCELL GDL 1500 0.059" 1.5 0.60 858 13.32 90.6 24.3
LINQCELL GDL 1500B 0.059" 1.5 0.60 670 21 140 39
LINQCELL GDL 1850 0.072" 1.85 0.85 1562 13.18 70.5 25.5
LINQCELL GDL 2900 0.011" 2.9 0.60 1734 24.57 87.7 27.6

All values are indicative and subject to tolerance

Spectracarb 2050A properties (Discontinued Q4 2021)
Product Thickness Thickness (mm) Density Required Loading for 12.5% ± 0.5% Strain Through-Plane Resistivity Standard size
Spectracarb 0850 .0075" ±.001"

0.19 ±0.02 0.5 g/cm³ ± 0.075 

100 lbf/in² ± 50

100 mOhm-cm @175 lbf/in² 16 x 16"
Spectracarb 1050 .011" ±.001" 0.28 ±0.02 0.5 g/cm³ ± 0.075  100 lbf/in² ± 50 100 mOhm-cm @175 lbf/in² 16 x 16"
Spectracarb 1550 .0145" ±.001" 0.37 ±0.02 0.5 g/cm³ ± 0.075  100 lbf/in² ± 50 100 mOhm-cm @175 lbf/in² 16 x 16"
Spectracarb 6060 .06" ±.005" 1.5 ±0.12  0.6 g/cm³ ± 0.075   300 lbf/in² ± 100 100 mOhm-cm @175 lbf/in² 22 x 22"
Spectracarb 7090 .064" ±.003" 1.6 ±0.07  0.775 g/cm³ ± 0.075   400 lbf/in² ± 150 100 mOhm-cm @175 lbf/in² 22 x 22"
Spectracarb 7090XT .084" ±.003" 2.1 ±0.07  0.775 g/cm³ ± 0.075   400 lbf/in² ± 150 100 mOhm-cm @175 lbf/in² 22 x 22"