Humiseal 1C49 | High Build, VOC-Free Silicone Conformal Coating

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

Humiseal 1C49 | High Build, VOC-Free Silicone Conformal Coating

Main features

  • VOC-free
  • High build
  • Fluoresces under UV light

Product Description

HumiSeal® 1C49 is a moisture-curing, high-build silicone conformal coating that offers exceptional moisture and environmental protection for printed circuit assemblies. This solvent and VOC-free coating is flexible, easy to inspect under UV light, and can be repaired. 1C49 can be cured at room or elevated temperatures.

Product Key Features

  • VOC-free and solvent-free for a safer application
  • High-build for excellent protection
  • Outstanding flexibility
  • UV light inspection for quality control
  • Repairable for easy rework
  • Recognized standards: MIL-I-46058C, IPC-CC-830, RoHS, and UL E105698

Applications

  • PCB applications with high build requirements.
Product Family

HS-1C49/5LC

5-Liter Can
1. Select Package Type

Loading pricing…

Product availability
EU Shipping in 12 weeks
Packaging
Unit of measure Bottle
Net weight 4.85 kg
Gross weight 5 kg
Dimensions 16.8 x 10.6 x 32 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
0.97 g/cm3
Solids
95 %
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
-65 °C
Operating Temperature
-65 - 200 °C
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V-1
Electrical Properties
Breakdown Voltage
Breakdown voltage is the minimum voltage necessary to force an insulator to conduct some amount of electricity. It is the point at which a material ceases to be an insulator and becomes a resistor that  conducts electricity at some proportion of the total current.  After dielectric breakdown, the material may or may not behave as an insulator any more because of the molecular structure alteration. The current flow tend to create a localised puncture that totally alters the dielectric properties of the material. This electrical property is thickness dependent and is the maximum amount of voltage that a dielectric material can withstand before breaking down. The breakdown voltage is calculated by multiplying the dielectric strength of the material times the thickness of the film.
7000 V
Other Properties
VOC-Free (100% solids content)
VOC means Volatile Organic compound. VOCs are evaporating molecules and are literally everywhere around us. Our scents are volatile organic compounds, most of the things that we smell are VOC etc. So what do we mean when we state that a product is VOC free? A VOC free product, according to the FTC is one where: 1)VOCs have not been intentionally added to the product. 2)The presence of VOCs at that level does not cause material harm that consumers typically associate with VOCs, including but not limited to, harm to the environment or human health. 3)The presence of VOCs at that level does not result in concentrations higher than would be found at background levels in the ambient air.
0
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
80-120 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
9000 mPa.s

Additional Information

Frequently Asked Questions About HumiSeal® 1C49

What are typical applications for HumiSeal® 1C49?

HumiSeal® 1C49 is a general-purpose, single-component, moisture-curing, high-build silicone conformal coating used for protecting printed circuit board assemblies (PCBs) in various industries, including:

  • Aerospace systems (e.g., avionics, control modules)
  • Automotive electronics (e.g., engine control units, sensors)
  • Industrial automation (e.g., motor drives, PLCs)
  • Consumer electronics (e.g., smartphones, gaming devices)

Why choose HumiSeal® 1C49 over other conformal coatings?

HumiSeal® 1C49 provides excellent protection, with outstanding flexibility and a VOC-free, solvent-free formulation. It provides excellent electrical insulation, fluoresces under UV for easy inspection, and is easily repairable with HumiSeal® Stripper 1091. It is also compliant with IPC-CC-830, MIL-I-46058C, and RoHS Directive 2011/65/EU, making it a trusted choice for demanding applications. You can learn how to select a conformal coating in our blog.

What is the shelf life of HumiSeal® 1C49?

HumiSeal® 1C49 has a shelf life of 12 months from the date of manufacture when stored at or below 27°C in tightly closed containers. Prior to use, allow the product to equilibrate for 24 hours at room temperature to ensure optimal performance.

How should I clean tools after applying HumiSeal® 1C49?

Tools and equipment used for applying HumiSeal® 1C49 (e.g., spray guns, brushes, or dipping tanks) can be cleaned with a suitable solvent, such as a mineral spirit or acetone, before the coating cures. Thinner is not required or recommended for this product. For removing the coating from PCBs during rework, use HumiSeal® Stripper 1091. Always use a lint-free cloth and ensure proper ventilation during cleaning.

What happens to HumiSeal® 1C49 after its shelf life?

Past its 12-month shelf life, HumiSeal® 1C49 may experience changes in viscosity, which could affect application consistency and coating uniformity. Using expired product may lead to suboptimal performance, and the manufacturer will not be liable for quality or performance issues if expired material is used. If the product has cured in the container, it cannot be recovered.

Why do curing times vary for HumiSeal® 1C49?

HumiSeal® 1C49 is a moisture-curing coating. Curing times vary depending on temperature, humidity, and film thickness. Typically, the coating will be tack-free in approximately 3 to 5 hours, and fully cured in 24 hours at room temperature. The full cure can be accelerated by using heat with an open pan of water to increase humidity, such as 20 minutes at 76°C.

What is the recommended thickness for HumiSeal® 1C49?

The recommended coating thickness for HumiSeal® 1C49 is 50 to 200 microns. This range ensures optimal protection without compromising flexibility or electrical performance. The thickness is controlled primarily by the application method and withdrawal rate, as the coating is not designed to be thinned.

What are the differences between application methods for HumiSeal® 1C49?

HumiSeal® 1C49 can be applied via spraying, dipping, or brushing. Spraying and dipping are ideal for large-scale production, while brushing is suited for small repairs. This product does not require thinning for any of these methods. Each method should be controlled to achieve a uniform coating, especially the withdrawal rate for dipping.

What is the maximum operating temperature for HumiSeal® 1C49?

HumiSeal® 1C49 can withstand thermal shock from -65°C to +200°C. It is also rated for continuous operation at 200°C, making it suitable for high-temperature applications where its protective properties must be maintained under constant thermal stress.

What safety precautions should I take when using HumiSeal® 1C49?

HumiSeal® 1C49 is VOC-free and solvent-free, reducing flammability risks. However, proper ventilation is still crucial to prevent inhalation of vapors or spray mist, especially since the coating cures via moisture in the air. Avoid skin and eye contact. Always consult the Safety Data Sheet (SDS) prior to use for detailed safety guidelines.

How can I ensure proper application of HumiSeal® 1C49?

HumiSeal® 1C49 fluoresces under UV light, allowing for easy inspection of coating coverage. After application, use a UV light source to check for a uniform, void-free coating, which is critical for high-reliability electronics manufacturing.

How does HumiSeal® 1C49 perform in harsh environments?

HumiSeal® 1C49 is designed for harsh conditions, with excellent fungus resistance per ASTM G21 and exceptional moisture insulation resistance. It maintains performance in humid, mechanically stressful, or temperature-cycling environments, making it ideal for mission-critical systems.

Learn More About HumiSeal® 1C49

HumiSeal® 1C49 is a proven solution for engineers seeking long-term protection of electronic assemblies in demanding environments. This silicone conformal coating offers a unique combination of ease of use, excellent electrical insulation, and exceptional flexibility—making it an industry favorite for protecting PCBs in sectors such as automotive, aerospace, consumer electronics, and industrial automation.

Key Features at a Glance

  • ✔ Tack-free in 3-5 hours at room temperature
  • ✔ High-build and 100% solids content
  • ✔ High-viscosity and VOC-free for easy application
Electrical protection 1C49
UV inspection 1C49

 


Versatile Application Methods 🧰

Application methods

Whether you’re using spraying, dipping, or brushing, 1C49 offers flexibility in manufacturing workflows. It is a 100% solids coating and should not be diluted. The coating cures at room temperature in 24 hours, allowing integration into both batch and inline processes.

Application Methods:

  • Spray: Apply using equipment for high-viscosity coatings
  • Dip: 5–15 cm/min withdrawal rate
  • Brush: For touch-up applications

Cure the coating at room temperature (24 hrs) for convenience, or accelerate with thermal curing to match fast-paced production cycles.

Application Compatibility

It integrates well with lead-free processes, supports standard cleaning practices, and offers strong performance even on flux-contaminated surfaces.

Compatible With:

  • ✔ Compatible with “no-clean” flux residues
  • ✔ Common PCB finishes including ENIG, HASL, and OSP
  • ✔ High-reliability applications requiring low ionic content
  • ✔ Lead-free and RoHS-compliant manufacturing environments
  • ✔ Cures at room temperature (24 hrs)

Additionally, its UV fluorescence ensures easy inspection, and the coating is reworkable using standard HumiSeal strippers—ideal for repairable designs and serviceable assemblies.


High-Performance Electrical Protection 🧪

1C49 delivers a dielectric breakdown voltage of 7,000 volts and an insulation resistance exceeding 5.0 x 1014 ohms, protecting even the most sensitive circuit designs from moisture, contaminants, and voltage-induced failure. It is rated for dielectric withstand voltage of >1,500 volts.

Fluorescent for Inspection 💡

To simplify quality assurance, HumiSeal® 1C49 fluoresces under UV light, making it easy to confirm proper coating coverage during post-application inspection—an essential feature for high-reliability electronics manufacturers.

Electrical protection 1C49
UV inspection 1C49

Repairable and Reworkable 🔁

Unlike many conformal coatings, HumiSeal® 1C49 is easily repairable. Should rework or component replacement be required, the coating can be selectively removed using HumiSeal® Stripper 1091, making it ideal for prototyping, low-volume builds, or field serviceability.

Reliable Across Environments 🌍

With a wide thermal shock range of –65°C to +200°C and resistance to fungus (ASTM G21) and moisture, 1C49 ensures consistent performance across varied environmental conditions. It’s particularly well-suited for mission-critical systems exposed to humidity, mechanical stress, or temperature cycling.


Compliance You Can Trust ✅

HumiSeal® 1C49 meets stringent industry standards, ensuring reliability and regulatory adherence for OEMs and contract manufacturers:

  • MIL-I-46058C Compliant
  • IPC-CC-830 Compliant
  • RoHS Directive 2011/65/EU Compliant
  • UL Recognized (File Number E105698).

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers