Hysol GR2310 | Gold Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

GR2310 Gold Epoxy Mold Compound Hysol GR2310 | Gold Epoxy Mold Compound

Main features

  • For MnO2 Tantalum Capacitors
  • Gold (yellow) colored
  • Halogen-free version MG33F-0520

Product Description

Hysol GR2310 is a Gold semiconductor epoxy molding compound or duroplast designed for the encapsulation and protection of Manganese Oxide (MnO2) tantalum capacitors and automotive sensor packages. Once molded and post-mold cured, this product provides optimium protection and reliability for these capacitor devices.

Hysol GR2310 is a laser markable product, designed for the new generation of capacitors. Tantalum capacitors are general purpose chip tantalum capacitors which are mature products and as such must be cost-competitive. Although the GR2310 has "only" been manufactured for 15 years or so, they are based on their halogen-containing counterparts and though these products do not contain halogens, the manufacturing process has been optimised a long time ago so as to offer the lowest cost possible.

Hysol GR2310 is an environmentally "green" product, meaning that doesn't contain any halogens including bromine, antimony or phosphorus flame retardants. MG33F-0520, MG33F-0588 and MG33F-0602 dominated the space for tantalum capacitors but used halogen-containing flame retardants. This next generation epoxy mold compound replaces these older generation products.This material is designed to achieve JEDEC Level 1 requirements at 260°C reflow temperature on Maganese Oxide MnO2 capacitors. Its fast cure time also ensures that it is compatible with the latest automold manufacturing equipment. Hysol GR2310 meets UL 94 V-0 Flammability at 1/4 inch (6.35mm) thickness.

Product Family

GR2310/14.3M4.4G15K

Pelletized - 14.3MM x 4.4GR | 15kg NET box
1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Box
Net weight 15 kg
Gross weight 16.5 kg
Dimensions 25.5 x 28.5 x 26.5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Gold
Filler Content
72 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.82
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
175 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.64 W/m.K
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V0
Physical Properties
Spiral Flow @ 175°C
72 cm
Mechanical Properties
Molded Shrinkage
0.28 %
Curing Conditions
Transfer Pressure
40 - 85 kg/cm2
Transfer Time
6 - 15 s