Hysol GR510 | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

GR 510 semiconductor epoxy molding mini-pellets QFP package Hysol GR510 | Black Epoxy Mold Compound GR510 Black Epoxy Mold Compound

Main features

  • High filler loading
  • Ultra low CTE of 8 ppm/°C
  • Designed for Quad Flat Pack (QFP) devices

Product Description

Hysol GR510 is a black, ultra-low CTE, transfer molded semiconductor epoxy molding compound designed for thin and larger quad flat pack (QFP) and larger small outline transistor (SOT) packages . Once transfer molded and post-mold cured, it has a very low CTE, low moisture absorption and high adhesion to a range of leadframe types. This allows it to acheive very high reliability levels for quad flat pack devices, but also for a range of larger SOIC packages.

Hysol GR510 has an ultra low coefficient of thermal expansion (CTE) of 8 ppm/°C that makes it one of the lowest stress materials avaiable in an epoxy molding compound. This low CTE comes from a technical breakthrough in filler size, filler type and filler loading. It has been successfully used for the production of printer heads from industry leading companies.

Hysol GR510 is an environmentally "green" product, meaning that it doesn't contain any bromine, antimony or phosphorus flame retardants. This material is designed to achieve JEDEC Level 1 requirements at 260°C reflow temperature on quad flat pack devices and other, larger small outline packages including SOT, SOD and SMX package types. Hysol GR510 meets UL 94 V-0 Flammability at 1/8 inch (3.175mm) thickness.

Product Family

GR510/C63J18

Pelletized - 25MM x 18GR | 15kg NET box
1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Box
Net weight 15 kg
Gross weight 15.51 kg
Dimensions 25.5 x 28.5 x 26.5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Black
Filler Content
88 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.99
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
30000000000000000 Ohms⋅cm
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
113 °C
Loss modulus peak @ DMA
111
Tan δ peak @ DMA
119
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V0
Chemical Properties
Moisture absorption
0.21 %
Curing Conditions
Transfer Pressure
40 - 85 kg/cm2
Transfer Time
5 - 15 s
Physical Properties
Spiral Flow @ 175°C
111.8 cm

Additional Information

GR510 is a product that can replace GR828-FC1 for power SOTs. FC initials might remind you of Fairchild. Fairchild has been acquired by Onsemi in 2017 so their products still live on.