SAC405 | Pb-free Solder Spheres

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

PMTC SAC405 Pb-free Solder Spheres SAC405 Pb-free Solder Spheres Tin-Lead (Pb) Phase Change Diagram

Main features

  • Pb-free Solder Spheres
  • Excellent Solder Joint Reliability
  • Best Wetting Sn/Ag/Cu Alloy

Product Description

LINQALLOY SAC405 solder Spheres are lead-free Tin/Silver/Copper alloys that contain 95.5% Tin (Sn), 4% Silver (Ag), and 0.5% Copper (Cu) and is often written as Sn95.5Ag4.0Cu0.5. SAC405 Solder Spheres are the more expensive of the two industry standard lead-free solder spheres (the other being SAC305) and are used by companies working with BGA, CSP, LBGA, PBGA and CBGA components who have made the transition to Lead-free (Pb-free) soldering.

Features:

  • Excellent Fatigue Resistance
  • Compatible with all Flux Types
  • Excellent Solder Joint Reliability
  • Best Wetting Sn/Ag/Cu Alloy

Each jar has a clear label on the lid specifying the solder ball diameter as well as a label on the front identifying the alloy type, the quantity of spheres in the jar, the date of manufacture, and the product lot (or batch) number. This batch number is also tied to a certificate of conformance that is also provided with the solder spheres and ensures the SAC405 solder spheres meet the following quality criteria:

  • Tin (Sn): 95.5%
  • Silver (Ag): 5%
  • Copper (Cu): 0.5%
  • Melting Temperature (Solidus): 217°C
  • Melting Temperature (Liquidus): 225°C
  • Sphericity : Within 1.5%

Diameter Tolerance

  • 0.22mm - 0.48mm (220µm - 480µm) : ± 0.010mm (± 10µm)
  • 0.50mm - 0.762mm (500µm - 762µm) : ± 0.025mm (± 25µm)
Product Family

SAC405/0.125-250kpcs

Alloy: Sn95.5/Ag4.0/Cu0.5 » 0.125mm (5mil) » 250,000 spheres
1. Select Diameter
2. Select Package Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Jar
Net weight 0.0019 kg
Gross weight 0.0021 kg
Dimensions 6 x 6 x 10 cm
TDS, SDS & Technical Documents

Technical Specifications

Other Properties
RoHS Compliant
RoHS is a product level compliance based on a European Union Directive which restricts the Use of certain Hazardous Substances in Electrical and Electronic Equipment (RoHS). Products compliant with this directive do not exceed the allowable amounts of the following restricted materials: lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls (PBB) and polybrominated diphenyl ethers (PBDE), with some limited exemptions
Yes
General Properties
Alloy Composition
Composition of the alloy material
Sn95.5Ag4.0Cu0.5
Alloy Type
A metallic element type
SAC405
Spheroid Tolerance
The allowed % that a solder ball (solder sphere) can divert from being perfectly round and spherical. We take one lot of solder spheres and divide it into 4 smaller lots. Each lot is then checked with advanced visual inspection systems. If even 1 ball is out of spec, the entire batch is scrapped and reworked!
1.5 %

Additional Information

What do I get when I buy SAC405 Solder Spheres from KRAYDEN?

The advantage of ordering solder spheres online at KRAYDEN.com is that you can be sure of the quality. The solder spheres you receive are originally manufactured solder spheres packed into jars with inert gas (nitrogen). We do not repack the solder balls we receive, so the jars you will receive have never been opened, thus ensuring the quality of the product you receive. The lid of the jar is also always sealed with a shrink-wrapped plastic wrap ensuring that the solder spheres do not oxidate in the jar.

 

Description Popular Brand1
Names
Competitive crossovers 
Leadfree (Pb-free) Tin Silver Copper (SAC) Solder Spheres. Compare the price and quality of other brands to LINQALLOY SAC405 Solder Spheres
  • Senju Sparkle Ball Sn95.5Ag4Cu0.5
  • Henkel Accurus Sn-Ag4-Cu0.5
  • Nippon Micrometal LF31
  • Cookson Alpha SAC405
  • Indium Precision Spheres 95.5Sn4Ag0.5Cu
  • Kester (EasySpheres) 10-4005
1 Sparkleballs®, Multicore Accurus®, Micrometal®, Precision Spheres®, Alphametal® and Ultra-Spheres® are registered trademarks of Senju, Henkel, NMC, Indium, Cookson and Kester respectively and are not affiliated with this site.

Presentation

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers