LINQCELL GDP210 | 210um Non woven Carbon Paper

Harmonization Code : 6815.11.00.00 | Articles of stone or of other mineral substances, not elsewhere specified or included; Non-electrical articles of graphite or other carbon; Carbon fibres and articles of carbon fibres

GDS210 | 210um Carbon Paper GDP210 | 210um Carbon Paper

Main features

  • 0.21mm - 210um - 8.2mil
  • Non woven
  • Roll form is possible.

Product Description

LINQCELL GDP210 is a 0.21mm thick non woven carbon paper without a Microporous layer and PTFE. It is commonly used as a gas diffusion layer and electrode for fuel cells. Its through-plane resistivity is less than 10 mΩcm2. This carbon paper is highly flexible and has excellent air permability.

LINQCELL GDP210 is a close alternative to the discontinued Spectracarb 0850. It is one of the few products that come in long roll form.

Product Family

GDP210/40M2R

m2 (40cm wide x 250cm long) | Roll
1. Select Sheet Size

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Roll
Net weight 0.0181 kg
Gross weight 0.02 kg
Dimensions 40 x 12 x 0.021 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Basis Weight
Basis weight refers to the weight measured in pounds off 500 sheets of paper in that paper’s basic sheet size.
50 g/m2
Other Properties
Air Permeability
10 seconds
Mechanical Properties
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
2 N/cm

Additional Information

LINQCELL GDP210 Properties

Property Value Unit
Thickness at 50 kPa 0.21 mm
Basis Weight 51 g/cm2
Air Permeability 3.3 s
Through-plane Resistance 10 mΩ⋅cm2
Voltage 14 mV

 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers