LINQCELL GDP250 | 250um Carbon Paper

Harmonization Code : 6815.11.00.00 | Articles of stone or of other mineral substances, not elsewhere specified or included; Non-electrical articles of graphite or other carbon; Carbon fibres and articles of carbon fibres

LINQCELL GDP250 | 250um Carbon Paper

Main features

  • 0.25 mm – 120 µm – 9.84 mil
  • Customizable with PTFE Coating and Available in Roll Form
  • Optimized as gas diffusion layers in fuel cells

Product Description

LINQCELL GDP250 is a 250-µm thick graphitized carbon fiber paper made from high-quality polyacrylonitrile (PAN) fibers. The fibers undergo a wet-laying process to form a non-woven, fibrous, and porous structure, which is then carbonized and graphitized at 1600 °C. This high-temperature graphitization results in high electrical conductivity, high oxidation resistance, and excellent thermal stability, making LINQCELL GDP250 highly recommended as gas diffusion layers in fuel cells. It can also be used as gas diffusion substrates for carbon dioxide electrolyzers. 

Key Features:

  • High-Temperature Graphitization: Graphitized at an elevated temperature of 1600 °C, this carbon fiber paper has a highly-crystalline graphite-like structure, enhancing conductivity, thermal stability, and oxidation resistance for demanding applications.
  • No MPL and PTFE Layer: Enables direct control of interfacial modifications for system-specific optimization in fuel cells and electrochemical devices.
  • High Permeability Despite Thickness ≥200 µm: Maintains high permeability for efficient gas diffusion and water management.

Highly Recommended As:

Due to the absence of a microporous layer, LINQCELL GDP250 exhibits high permeability despite its thickness (≥200 µm). This makes it particularly well-suited for high-humidity fuel cell operation (≥60%) at temperatures between 50 and 80 °C. In medium humidity conditions (20 to 60%), LINQCELL GDP250 may perform effectively, but the temperature should be kept low (≤50 °C).

Recommended For Fuel Cells Operating at:

  • High humidity (≥60%) at temperatures between 50 to 80 °C
  • Medium relative humidity (20 to 60%) at low temperatures ≤50 °C

LINQCELL GDP250 can be customized to meet specific requirements. It can be coated with a 10 wt% PTFE layer and is also available in roll form.

Product Family

GDP250/40X40

40 x 40cm Sheet
1. Select Sheet Size

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Sheet
Net weight 0.064 kg
Gross weight 0.0704 kg
Dimensions 40 x 40 x 0.025 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Basis Weight
Basis weight refers to the weight measured in pounds off 500 sheets of paper in that paper’s basic sheet size.
65 g/m2
Porosity
Void fraction is a measure of the void spaces in a material
77 %
Electrical Properties
TP Resistance
Opposition to the flow of electric current.
6 mΩcm2
Other Properties
Air Permeability
10 seconds
Mechanical Properties
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
24/22 N/cm

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers