LOCTITE 3217

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 3217

Main features

  • UV & Heat Cure
  • Non Conductive
  • Image sensor module assemblies

Product Description

LOCTITE 3217 dual cure adhesive is designed for use in the assembly of temperature sensitive electronic components. The maximum performance of this material is achieved by exposure to UV light of sufficient intensity, followed by thermal cure.

LOCTITE 3217 dual cure epoxy/acrylate (UV and heat) is an amber high viscosity material that is used for optical applications and the cavity fill of test IC's. It has good adhesion on glass and metals, based on customer experiences and it has been successfully used for Automotive applications.

 

UV Cure

  • Medium pressure mercury lamp UV Wavelength, nm 220 to 260
  • Light Intensity, mW/cm² 100
  • UV Tack-Free Time, seconds 1

Heat Cure

  • 30 minutes @ 60°C
  • 25 minutes @ 70°C
  • 20 minutes @ 80°C
Product Family

3217/50U0

50cc MUS Syringe - 915160
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 53 days
CA Shipping in 12 weeks
EU Shipping in 45 days
Packaging
Unit of measure Syringe
Net weight 50 g
Gross weight 82 g
Dimensions 4.5 x 3 x 16 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
336 hours
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.2
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
82 °C
Physical Properties
Thixotropic index
Thixotropic Index is a ratio of a material s viscosity at two different speeds in Ambient temperature, generally different by a factor of ten. A thixotropic material s viscosity will decrease as agitation or pressure is increased. It indicates the capability of a material to hold its shape. Mayonnaise is a great example of this. It holds its shape very well, but when a shear stress is applied, the material easily spreads. It helps in choosing a material in accordance to the application, dispense method and viscosity of a material.
2.9
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
109,000 mPa.s

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers