PCM 45F | Phase Change Pad
Harmonization Code : 8547.90.00.00 | Insulating fittings for electrical machines, appliances or equipment, being fittings wholly of insulating material apart from any minor components of metal (for example, threaded sockets) incorporated during moulding solely for purposes of assembly, other than insulators of heading 8546; electrical conduit tubing and joints therefor, of base metal
Main features
- 0.09 - 0.12 Thermal Impedance
- 2.0 - 2.5 Thermal Conductivity
- Pad form
Product Description
PCM45F is Honeywell's thermally conductive phase change pad. It is designed to minimize thermal resistance at interfaces and maintain extremely stable performance through reliability testing required for long product life applications. In addition to that it has excellent electrical properties and very high volume resistivity.
PCM45F has a Thermal conductivity of 2.0 - 2.5 (W/m·K) depending on the bondline thickness and is based on a robust polymer PCM structure that exhibits excellent wetting properties during typical operating temperature ranges, resulting in very low surface contact resistance. The proprietary material provides superior reliability and maintains low thermal impedance (0.09-0.12) , making it desirable for high-performance integrated circuit devices.
Packaging
Unit of measure Sheet
Net weight 0.04 kg
Gross weight 0.04 kg
Dimensions 0.03 x 15 x 40 cm
Technical Specifications
General Properties
Specific Gravity
2.2
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume.
For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
Thickness range
0.20 - 1.00 mm
Thermal Properties
Thermal Conductivity
2.0 - 2.5 W/m.K
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance.
Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
Thermal Impedance
0.09 - 0.12 °C·cm²/W
Electrical Properties
Volume Resistivity
820000000000000 Ohms⋅cm
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
Additional Information
When choosing a printable paste it is important to understand the process parameters and limitations.
That's why we ask, when you contact us, to include the following information:
- What is your print thickness?
- How long is your printing time and working window?
- What is your drying step after printing?
- Temperature (Room temperature or something else?)
- Time
- Do you have any viscosity limitations in the printing process?