PTM 5000 | Phase Change Pad

Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other

PTM5000 | Phase Change Pad

Main features

  • 0.06 - 0.08 Thermal Impedance
  • 3.5 - 4.5 Thermal Conductivity
  • Pad form

Product Description

PTM5000 is Honeywell's thermally conductive phase change material in pad form. Admittedly it is the most effective, all around solution in Honeywell's phase change portfolio. It is designed to minimize thermal resistance at interfaces and maintain extremely stable performance through reliability testing required for long product life applications.

PTM5000 has a Thermal conductivity of 3.5 - 4.5 (W/m·K) depending on the bondline thickness and is based on a robust polymer PCM structure that exhibits excellent wetting properties during typical operating temperature ranges, resulting in very low surface contact resistance. The proprietary material provides superior reliability and maintains low thermal impedance (0.06-0.08) , making it desirable for high-performance integrated circuit devices. Clamping pressure and temperature are suggested to achieve a minimum bondline thickness for the best performance. All information for Thermal impedance is collected after the product is fully phase changed and without a shim.

Product Family

PTM5000/025P0

52.5 x 52.5 x 0.25mm Pad
1. Select Package Type

Loading pricing…

Product availability
EU Shipping in 8 weeks
Packaging
Unit of measure Pad
Net weight 1.584844 g
Gross weight 1.584844 g
Dimensions 5.25 x 5.25 x 0.03 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
2.3
Thickness range
0.20 - 1.00 mm
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
3.5 - 4.5 W/m.K
Thermal Impedance
0.06 - 0.08 °C·cm²/W
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
210000000000000 Ohms⋅cm

Additional Information


BLT Vs Pressure Curve @80°C

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers