PTM 7000-SPM | Phase Change Paste
Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other
Main features
- 0.06 Thermal Impedance
- 6.5 Thermal Conductivity
- Medium drying solvent
Product Description
PTM7000-SPM is identical to PTM7000-SP but with a medium drying solvent for processes that require longer drying time. This means that drying time is ±48 hours at room temperature and ±8minutes at 100°C. It is designed to minimize thermal resistance at interfaces and maintain extremely stable performance through reliability testing required for long product life applications. As with all Phase change materials, it has stable Thermal Impedance across accelerated aging tests and does not display bleed, pump or flow out. SPM-Medium drying solvents are nice to have but SP versions should work just as well since the initial drying up issues are usually cleared up quickly after the printing equipment setup has been optimised.
PTM7000-SPM has a Thermal conductivity of 6.5 (W/m·K) depending on the bondline thickness and is based on a robust polymer PCM structure that exhibits excellent wetting properties during typical operating temperature ranges, resulting in very low surface contact resistance. This proprietary material provides superior reliability and maintains low thermal impedance (0.06) , making it desirable for high-performance integrated circuit devices. Its latent heat of fusion is 0.62 J/g while its Specific heat capacity is 0.96 J/g.
Solvent Drying time:
- 48hours @ 23°C
- 8mins @ 100°C
Packaging
Technical Specifications
General Properties
Thermal Properties
Electrical Properties
Physical Properties
Additional Information
SPM Solvent System Designed for Longer Processing Time
Solstice PTM7000-SPM incorporates a modified solvent system specifically designed to provide an extended processing window compared with the standard PTM7000-SP formulation. Its slower solvent evaporation rate allows the material to maintain its workable consistency for a longer period, offering greater flexibility during dispensing, stencil printing, and other paste application processes.
The optimized solvent system is particularly beneficial for manufacturing operations involving extended processing cycles, larger application areas, or intermittent production, where premature solvent evaporation could affect paste consistency and application uniformity.
The drying profiles of PTM7000-SP and PTM7000-SPM at 23°C demonstrate a significant difference in their initial solvent evaporation rates:
The standard PTM7000-SP formulation exhibits relatively rapid initial solvent evaporation, reaching approximately 5% weight loss within the first 6 hours. In comparison, PTM7000-SPM demonstrates a more gradual drying profile, with approximately 3% weight loss after 6 hours. The formulation reaches approximately 5.5% weight loss after 24 hours, indicating a slower and more controlled solvent evaporation process.
Both formulations eventually reach a similar total weight loss of approximately 5.8% after 48–72 hours, suggesting comparable overall volatile content despite their different drying kinetics.
Extended Processing Window with Accelerated Drying at 100°C
Despite its slower evaporation behavior at room temperature, PTM7000-SPM also demonstrates accelerated solvent removal when exposed to elevated temperatures.
At 100°C, PTM7000-SPM reaches approximately 4.5% weight loss after 10 minutes, increasing to approximately 6.0% after 30 minutes. The weight loss subsequently approaches 6.5% after 60 minutes, with minimal additional change observed through 120 minutes.
These results demonstrate that elevated-temperature drying can substantially accelerate solvent evaporation after application, potentially reducing the drying time required under ambient conditions.
Printable Paste Guidelines
When choosing a printable paste it is important to understand the process parameters and limitations.
That's why we ask, when you contact us, to include the following information:
- What is your print thickness?
- How long is your printing time and working window?
- What is your drying step after printing?
- Temperature (Room temperature or something else?)
- Time
- Do you have any viscosity limitations in the printing process?

PTM7XXX Series - Pressure vs Thermal Impedance
PTM7XXX Series vs Competition comparison (lower is better)
What is shelf-life and the shelf-life of the PTM7000-SPM?
Shelf-life refers to the amount of time the material can be kept when stored under the recommended storage conditions. The shelf-life of the PTM7000-SPM is 12 months when kept below 25°C and with less than 20% relative humidity (RH).
How is the material prepared prior to use?
If the material is supplied in 280cc cartridges, then the PTM7000-SPM can be dispensed directly onto the stencil. If the PTM7000-SPM is supplied in 1kg can, then it is best to mix or roll the material prior to each use. "Rolling" involves simply having the material "self-mix" which the can is being rolled (for this there is standard "jar roller" equipment).
Which packaging, the 1kg can or the 280cc aluminum cartridge is best recommended to use?
This depends on how you plan to apply the material. If you plan to dispense from a cartridge (hardly anyone dispenses) using a nozzle, then a cartridge is recommended. Also, if you plan to do much smaller batch sizes (ie less then 1kg at a time), then 280cc cartridges are better because you will lose less material per use. Printing, however, is a high throughput process. On any print cycle you will need at least 100cc of material on the stencil during printing which can coat many pieces per stroke. You will easily use up 280cc of material per shift during printing.
What is the potlife of the PTM7000-SPM?
Potlife (also referred to as work life) refers to the amount of time the material can be still be used after it has been opened. When kept in the 1kg cans, the potlife is 12 hours from the time the can is opened. When the lid is replaced and the can is closed again, you will have 48 hours to use the balance of the material. The remaining material should also be remixed (or re-rolled on a jar roller) prior to use.
Similarly, in the 280cc cartridge, the potlife is 24hrs if dispensed from the cartridge directly. If the cartridge is opened to add material to the printer and then closed again, the balance of the material should be used within 24-36 hours.
What is the thickness difference before and after drying?
It is typical to lose approx. 20% thickness due to solvent drying. For example, a 300µm (0.3mm) thickness stencil of wet PTM7000-SPM will result in 240µm (0.24mm) after drying. If the thickness loss is more than 20%, then the can was not stirred or rolled and it is indicative of mixing issues prior to dispensing them on the printing equipment.
PTM7000-SPM can dry completely when it is baked for 8 minutes at 100°C (based on 0.1 BLT). Thicker bondlines will require more time and temperature. For example for a 0.5mm sample fully dries after 15minutes at 140°C. It starts with ±15% shrinkage at 5 minutes and keeps on shrinking until it reaches ±21% at 15 minutes, after the solvent is fully dried.
What should I know about the Flash Point of this material?
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source. For SPM, the solvent content is under 10% of the formulation. The flashpoint of the solvent is more than 50℃ and its boil point is more than 180℃. Thus, the solvent steam at room temperature is relatively safe and has a very low risk of combustion. As long as there is no open fire in the oven and have a good ventilating system that can let solvent steam from the oven into the environment, the solvent in the material during the drying process will be very safe.
If your oven is not of the latest technology and you need to consider the flammable limits, the lower one is 0.6% and the upper one 6.0%