TGP 3510PT | Thermal Putty Pad

Harmonization Code : 3824.99.96.99 | Prepared binders for foundry moulds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included : Other : Other: Other

TGP 3510PT | Thermal Putty Pad

Main features

  • 0.45 Thermal Impedance
  • 3.5 Thermal Conductivity
  • 0.5 - 5 mm Thickness

Product Description

Honeywell TGP 3510PT is a green, thermally Conductive Putty Pad that provides high thermal performance and excellent thermal reliability. The material’s putty-like design enables excellent gap-filling capability for applications with large dimensional variances. Special surface reinforcement enables easier handling for operators during high volume assembly. It comes packaged with single (>=1mm) or double (<1mm) sided fiber glass  and dual liners. 

Honeywell TGP 3510PT is naturally tacky and requires no additional adhesive to mate to heat source and heat sink. This product can improve production efficiency by replacing pre cured gels and is available in thicknesses ranging from 1.0mm to 5.0mm.

Need a thickness below 1mm? Then we recommend our standard Thermal gap pads.

Product Family

TGP3510PT/1P0

457 x 457 x 1.0mm Pad
1. Select Package Type

Loading pricing…

Product availability
EU Shipping in 16 weeks
Packaging
Unit of measure Pad
Net weight 0.67 kg
Gross weight 0.74 kg
Dimensions 45.7 x 45.7 x 0.1 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Green
Film Thickness
Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
0.5 - 5 mm
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
3.2
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
3.5 W/m.K
Thermal Impedance
0.45 °C·cm²/W
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V-0
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
40000000000000 Ohms⋅cm

Additional Information

Fiberglass Layer Feature

Since these are ultra-soft materials, handling during application presented certain challenges. To improve stability and ease of processing, a double layer of fiberglass reinforcement was added.






 

 

Shelf Life: 12 months at 23±2˚C

Thickness range: 1.0-5.0mm with 0.25mm incremental

Thickness Tolerance: >=1mm, ±10%, 0.5-1mm, ±0.1mm

What is the difference between TGP3500PT and TGP3510PT?

The key differences between these two grades are color and quality control.

  • Color
    • In the figure below you can see that TGP3510PT is green, meanwhile TGP3500PT is white.
  • Quality control
    • The hardness of both is exactly the same during the quality test. Specs for both grades are 6-20.
    • The residual stress of TGP3500PT (@70% compression)is its QA item and it will be tested for each lot. This data is listed on COA as one of the quality items.
    • Oil bleeding of TGP3500PT is tested every 5 lots. Test result is used as HON internal control but this is not listed in COA.

 

 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers